Visitor No. 295002
Test Report
Bennewart Flexing Test
Observation
No Significant Cut Growth Observed at 30,000 Cycles
Requirements
6mm (max) cut growth after 30,000 cycles
Abrasion Resistance
Volume Loss in mm 3
97 mm3
Requirements
300 mm3 (maximum)
Ross Flex after Hydolysis
Observation
1 mm cut growht was observed in sample till 15,000 cycles
Requirements
4 mm(max) cut growth after 15,000 cycles